Differential Scanning Calorimetry, commonly known as DSC, is a thermo-analytical technique for polymeric and non-metallic materials. Most commonly used for detecting glass transition temperature and other thermal properties, differential scanning calorimetry is one of the most efficient and cost-effective polymer test methods available.

 

Differential scanning calorimetry testing

DSC testing has been used for decades as a way to predict the behaviors of polymeric materials under different thermal conditions. Like all calorimeters, this technique tracks the amount of energy required to increase the temperature of a material by a certain amount. By making accurate measurements of heat capacity and temperature, differential scanning calorimetry can detect changes in material properties at exact temperatures, revealing important transition ranges and deterioration points.

 

How is DSC testing performed?

To perform DSC testing, a small amount of material is heated at a predetermined rate. The energy required to heat the sample is compared to an inert reference material at the same temperature. If the sample under test requires more energy compared to the reference, it is indicated as an endotherm. The peak of an endotherm indicated melting temperature. When less energy is required to heat the sample as compared to the inert reference, an exothermic peak is observed. This may indicate a chemical reaction such as curing is taking place. 

 

Hassle-free testing to a range of standards

American Society of Testing & Materials

ASTM D3417, ASTM D3418, ASTM D3895, ASTM D4591, ASTM D7426, ASTM E1131, ASTM E1269, ASTM E1356, ASTM E1858, ASTM E2160, ASTM E2602, ASTM E793, ASTM E794, ASTM E831, ASTM F1514, ASTM F262

Deutsches Institut für Normung

DIN 51007, DIN 75201

Institute for Interconnecting and Packaging Electronic Circuits

IPC-TM-650

International Standards Organization

ISO 11357, ISO 11358, ISO 11359

Various Customer Specifications

SRM 25R-94, PA-06, PA-14, GM 9094P, MAP N215

 

Why choose 国产偷拍自拍?

国产偷拍自拍 performs DSC testing in laboratories across the US and Europe. Our polymer testing experts have years of experience across a variety of industries, and can help you overcome the unique challenges inherent with non-metallic materials. Contact an expert today to let us know how we can make your next project a success.

Ready to request a quote?

Our deliverable is certainty - high quality data, test reports and certificates that you can absolutely rely on when making decisions about your materials and compliance. Engage with an expert today.

Our team of over 9,000 Engaged Experts in North America, Europe, The Middle East, Australia, Asia and Africa are ready to help you.